Dx55d+As120 알루미늄 도금 강철 튜브

설명

DX55D+AS120 combines a formable EN 10346 steel substrate with an aluminum-silicon coating. It is designed for applications that need good cold forming, stable mechanical properties, and better heat and oxidation resistance than uncoated carbon steel. 하지만, one point should be clarified before purchasing: DX55D is not a 500 MPa yield-strength steel. Under EN 10346, DX55D has a typical proof/yield strength range of about 140–240 MPa and tensile strength of 270–370 MPa. The “550 MPa” level belongs to grades such as S550GD, not DX55D.

Quick answer: DX55D+AS120 is best understood as a high-formability cold-forming substrate + medium Al-Si coating. It is suitable for thin-wall formed tubes, exhaust-related components, heat-exposed parts, agricultural equipment, and selected automotive components where formability and coating performance must work together.

What Does DX55D+AS120 Mean?

The designation contains two separate material requirements. DX55D identifies the steel substrate according to EN 10346. The “D” family is associated with continuously hot-dip coated flat products for cold forming. +처럼 identifies an aluminum-silicon coating, ~하는 동안 AS120 indicates a coating-weight class of approximately 120 g/m² total for both sides, subject to the applicable standard, 용인, and supply agreement.

DesignationMeaning주요 기능
DX55D안에 10346 cold-forming steel gradeFormability and substrate strength
+처럼알루미늄-실리콘 코팅Heat and oxidation resistance
AS120대략. 120 g/m² coating classMedium coating protection

DX55D Is a Forming Grade, Not a 500 MPa Yield Grade

This distinction is important when a tube is specified for structural loading. DX55D belongs to the cold-forming grade family. Its mechanical properties are quite different from a 500 MPa structural steel.

For DX55D+AS products in the EN 10346 data published by ArcelorMittal, the proof/yield strength is about 140–240 MPa, tensile strength is 270–370 MPa, and the minimum A80 elongation is generally 30% for thicknesses from 0.7 에게 3 mm. Lower minimum elongation values can apply to thinner products.

재산DX55D+AS referencePurchasing note
Proof/yield strength, Re/Rp0.2140–240 MPaNot a 500 MPa-class yield steel
인장강도, Rm270–370 MPaVerify against the mill certificate
A80 elongation≥30% at 0.7–3 mmThickness affects the minimum value
코팅AS120 classConfirm coating-weight basis and tolerance

Important specification check: If your engineering drawing really requires a ~500 MPa yield strength, DX55D should not be substituted without engineering approval. A structural grade such as S550GD is a different material category and should be specified separately.

How Does the DX Grade Strength Ladder Work?

The DX51D–DX57D sequence is often misunderstood as a simple strength ladder. In reality, these grades are primarily differentiated by cold-forming performance, not by a simple increase in yield strength. As the grade moves toward DX56D and DX57D, formability generally becomes more demanding and elongation requirements increase. DX55D is therefore better described as a strong-formability grade rather than a high-yield structural grade.

등급General positioningTypical purpose
DX51DGeneral formingSimple formed parts
DX52DImproved formingMore demanding forming
DX53DDeep-forming levelDeeper formed components
DX54DVery good formabilityComplex cold forming
DX55DSpecial cold-forming gradeFormed parts requiring controlled properties
DX56D / DX57DHigher formabilityMore demanding forming applications

Why Combine DX55D with AS120?

The value of this combination comes from using different material features for different jobs. 그만큼 DX55D substrate provides cold-forming capability, 동안 AS120 coating provides an aluminum-silicon surface that is useful where heat and oxidation resistance are important.

For thin-wall tube production, this can provide a practical balance. The substrate can be roll formed or otherwise shaped before the tube is finished, while the coating helps protect the surface during elevated-temperature service.

DX55D

Cold-forming performance, 연성, and controlled substrate properties.

AS120

Medium Al-Si coating for heat and oxidation protection.

Finished Tube

A formed thin-wall product for selected industrial service conditions.

Example Specifications for DX55D+AS120 Tube

Tube dimensions depend on the forming route, 애플리케이션, and equipment. The following are practical example ranges rather than universal EN 10346 튜브 치수.

목Example specification메모
재료DX55D+AS120EN 10346-based substrate/coating designation
Outside diameter20–60 mmExample range for thin-wall tube programs
벽 두께0.8-2.0mmConfirm according to load and forming process
코팅 클래스AS120Confirm actual coating mass by inspection
표면Al-Si coatedAppearance depends on production route
Supply formStraight tube or cut lengthCustom lengths can be discussed

Where Is It Used?

농업 기계 is one potential application. Equipment such as tractors, harvesters, implements, guards, 덕트, and exhaust-related components can require a combination of low weight, forming capability, and resistance to heat or oxidation.

Automotive components are another important area. Depending on the design, the material can be considered for exhaust-related tubes, 열 차폐, air or fluid routing components, 괄호, and other formed parts. The exact application must be checked against temperature, load, 부식 환경, and joining requirements.

It can also be considered for selected industrial equipment, HVAC 구성 요소, heat-transfer systems, and other thin-wall products where an Al-Si surface is preferred over ordinary uncoated carbon steel.

Welding Considerations

Do not treat DX55D as a conventional 500 MPa high-strength steel that automatically requires heavy preheating. Its EN 10346 mechanical properties are much lower than that description suggests. Welding should instead focus on the actual thickness, joint design, 용접 공정, heat input, and the Al-Si coating.

The coating is the main practical issue. Welding can locally remove or damage the aluminum-silicon layer. Fumes must also be controlled with suitable ventilation and extraction. Where the coating is removed around the weld zone, the exposed steel should be considered for suitable post-weld protection if the service environment requires it.

Welding issueRecommended approach
Al-Si coating near weldControl the weld zone and avoid unnecessary coating damage
Fume generationUse effective local exhaust ventilation
Thin-wall burn-throughUse controlled heat input and suitable parameters
Post-weld corrosionInspect exposed areas and apply an approved repair/protection method when required
Structural loadingVerify actual substrate strength rather than assuming “DX55D” means 500 MPa yield

DX55D+AS120 vs a Higher-Strength Structural Grade

The material should be selected according to the real design requirement. If the main priority is forming a thin-wall tube, DX55D can be attractive. If the main requirement is a high structural yield strength, a structural grade such as S350GD or S550GD may be more appropriate, depending on the design. 안에 10346 lists S550GD at a minimum proof strength of 550 MPa and minimum tensile strength of 560 MPa.

Design rule: Do not choose the grade from the coating name alone. Specify the required 기질 등급 + coating class + 튜브 치수 + mechanical properties + 성형방법 + service temperature.

Buying Checklist for DX55D+AS120 Tube

  • Confirm that DX55D is actually required for cold forming, rather than assuming it is a 500 MPa structural steel.
  • Specify AS120 and confirm the coating-weight basis, 용인, and inspection method.
  • Define outside diameter and wall thickness clearly.
  • Request the mill test certificate for substrate chemistry and mechanical properties.
  • Check coating quality before tube forming and after forming.
  • For welded tubes, define the welding process and post-weld coating protection.
  • For automotive or agricultural applications, provide the working temperature and corrosion environment before final grade approval.

DX55D+AS120 Tube Supply from Teda Ganghua

Teda Ganghua can support industrial buyers sourcing Al-Si coated steel tube materials from China. For projects requiring a balance of forming performance and coating protection, the material can be evaluated according to tube diameter, 벽 두께, coating class, application temperature, and required mechanical properties.

As a metal supplier, Teda Ganghua can also help coordinate related processing requirements such as cutting, 형성, 용접, and customized tube supply. For buyers comparing different Al-Si coating levels, 우리의 알루미늄 도금 강철 튜브 range can be matched to the required substrate and service environment.

For a project inquiry, it is useful to provide the required grade, AS coating level, 의, 벽 두께, 튜브 길이, 수량, end condition, welding requirement, 및 적용. This allows the specification to be checked before quotation.

FAQs

Is DX55D a 500 MPa steel?

아니요. Under EN 10346, DX55D has a proof/yield strength range of about 140–240 MPa and tensile strength of about 270–370 MPa. 에이 550 MPa minimum yield level is associated with S550GD, not DX55D.

What does AS120 mean?

AS120 refers to an aluminum-silicon coating-weight class of approximately 120 g/m² total for both sides, subject to the applicable standard and agreed tolerances. The exact delivered coating should be verified against the purchase specification.

Is DX55D+AS120 suitable for automotive exhaust components?

It can be considered for selected exhaust and heat-exposed components. Final suitability depends on temperature, 열 순환, 부식 조건, tube geometry, 용접 방법, 및 필요한 서비스 수명.

Does DX55D+AS120 require preheating before welding?

단순히 DX55D라고 해서가 아니다.. 그것은 아니다 500 MPa급 고강도 기판. 용접 매개변수는 두께에 따라 선택되어야 합니다., joint design, 프로세스, heat input, Al-Si 코팅에 대한 용접 효과.

이 튜브를 주문할 때 지정해야 할 사항?

기판 등급 지정, AS120 코팅 클래스, 외경, 벽 두께, 튜브 길이, 기계적 요구 사항, 표면 요구 사항, 용접조건, 수량, 그리고 의도한 서비스 환경. 이러한 세부정보는 튜브의 상품명만 지정하는 것보다 더 신뢰할 수 있습니다..

Al-Si 코팅 강철 튜브

Al-Si 합금 코팅 강관