Panduan Salutan Tiub Keluli Beralumi AS120 AS150 AS200

Panduan Salutan Tiub Keluli Beralumi AS120 AS150 AS200

AS120, AS150, dan AS200 adalah sebutan jisim salutan, bukan penilaian suhu. Untuk tiub keluli beraluminium, the number generally indicates the specified coating mass per unit area, so a higher designation means a heavier metallic coating. This distinction is important in high-temperature applications: increasing coating mass can improve coating durability and provide more material for corrosion protection, but it does not automatically make a tube suitable for a higher operating temperature. The base steel grade, sistem salutan, atmosphere, tube geometry, berbasikal haba, and required service life must be considered together.

What Do AS120, AS150 and AS200 Mean?

Dalam spesifikasi keluli alumin, AS designations are commonly used to identify the coating mass. AS120, AS150, and AS200 therefore represent progressively heavier coating levels. The exact measurement convention and minimum requirements should always be confirmed against the applicable product standard and purchase specification.

GredNominal coating-mass designationGeneral positioningTypical selection logic
AS120About 120 g/m² total coating massCommon general-purpose levelBalanced coating requirement and forming/processing needs
AS150About 150 g/m² total coating massHeavier coating levelGreater coating reserve where exposure or service demand increases
AS200About 200 g/m² total coating massHeavy coating levelApplications requiring a larger coating allowance, subject to forming and specification limits

The stated coating mass is normally a mass-per-area requirement, not a direct coating-thickness specification. Actual coating thickness depends on coating density and measurement method. Buyers should therefore avoid converting AS120, AS150, or AS200 into a fixed micrometer value without checking the governing standard.

Does a Higher AS Grade Mean Higher Temperature Resistance?

Not by itself. This is one of the most important points when selecting aluminized steel tubes for furnaces, sistem ekzos, saluran udara panas, ketuhar, penunu, and other elevated-temperature applications.

AS200 does not mean “200°C” and AS150 does not mean “150°C.” The numbers identify coating mass rather than the maximum service temperature.

Pada suhu tinggi, the aluminum-silicon coating develops an intermetallic diffusion layer with the steel substrate. The coating can provide strong resistance to oxidation and corrosion, but prolonged exposure, berbasikal haba, mechanical deformation, coating damage, and the surrounding atmosphere all influence actual service life.

AS120 vs AS150 vs AS200 for High-Temperature Service

For high-temperature tube procurement, the selection should start with the environment rather than simply choosing the largest coating number.

AS120

A practical choice where the coating requirement is moderate and the tube is not subjected to unusually severe external corrosion or repeated coating damage. It is also widely used where forming and processing efficiency are important.

AS150

A heavier coating provides additional coating reserve. It can be considered when the environment or expected service duration creates a stronger requirement for coating protection, provided the forming process is compatible.

AS200

The heavier coating level can be specified when additional coating mass is required by the application or purchasing standard. It should not be selected solely because the operating temperature is high.

The Five Factors That Matter More Than the AS Number

1. Operating Temperature

Determine the normal temperature, suhu puncak, tempoh pendedahan, and frequency of thermal cycling. A tube experiencing short peaks is not exposed in the same way as one operating continuously at an elevated temperature.

2. Atmosphere

Combustion gases, oxygen-rich air, lembapan, garam, sulfur-bearing gases, condensate, and other contaminants can change coating behavior. A material suitable for dry hot air may require a different specification in a corrosive combustion environment.

3. Base Steel Grade

The coating is only one part of the tube system. Base-metal strength, creep behavior, rintangan pengoksidaan, forming characteristics, and thermal expansion must be considered at the intended operating temperature.

4. Tube Processing

Membongkok, memotong, menyala, mengimpal, piercing, and end forming can locally damage or redistribute the coating. A heavier coating does not eliminate the need to control coating integrity after fabrication.

5. Required Service Life

Two tubes operating at the same temperature may require different coating levels because their exposure duration, persekitaran kakisan, and maintenance cycles are different.

High-Temperature Application Mapping

PermohonanMain concernCoating selection approach
Komponen ekzos automotifThermal cycling and oxidationSelect coating and base steel together; validate the actual exhaust temperature profile
Hot-air ductsContinuous heat and external corrosionAS120–AS200 may be considered according to exposure and service-life requirements
Oven and baking equipmentSuhu, cleanliness, and coating integrityConfirm the coating and substrate are appropriate for the equipment and contact environment
Industrial heating systemsHigh temperature plus thermal cyclingSpecify operating profile, atmosphere, base steel, coating mass, and testing requirements
General fabricated tubingForming and coating damageChoose the coating level together with bending and welding requirements

What Should Be Written on the Purchase Order?

Writing only “aluminized steel tube AS120” leaves several important variables undefined. A technical inquiry should identify the complete tube specification.

Recommended inquiry information:

How to Choose Between AS120, AS150 and AS200

A simple procurement decision can be organized around three questions:

  1. Is AS120 already sufficient under the applicable specification and service environment? If yes, increasing coating mass may not provide a meaningful benefit.
  2. Does the environment justify additional coating reserve? If exposure is more demanding, AS150 or AS200 can be evaluated according to the required standard and forming conditions.
  3. Is the actual limitation temperature rather than corrosion protection? If the concern is maximum service temperature, changing from AS120 to AS200 may not solve the problem. The base steel and complete material system must be reviewed.

Teda Ganghua Aluminized Steel Tube Supply

Teda Ganghua supports aluminized steel tube sourcing for applications requiring controlled tube dimensions, spesifikasi salutan, and customized supply. Procurement can be organized around tube OD, ketebalan dinding, panjang, coating level, bahan asas, internal coating requirements, pemprosesan, kuantiti, and delivery schedule.

For buyers comparing AS120, AS150, and AS200, Teda Ganghua can help match the tiub keluli beraluminium specification with the intended service environment rather than treating the coating number as a temperature rating. Submit the required dimensions, coating mass, keadaan operasi, and applicable standard for a technical quotation.

Tiub keluli beraluminium can be reviewed for different industrial tube requirements and customized procurement specifications.

For a high-temperature tube inquiry, send:

DARIPADA + ketebalan dinding + panjang + gred keluli asas + AS coating level + internal coating requirement + suhu operasi + atmosphere + kuantiti + piawaian yang berkenaan.

FAQs About AS120, AS150 and AS200

Does AS200 mean the tube can operate at 200°C?

Tidak. AS200 refers to a coating-mass designation, not a 200°C service-temperature rating. Maximum service temperature must be evaluated from the complete material specification and application conditions.

Is AS200 always better than AS120 for high-temperature applications?

Tak semestinya. A heavier coating can provide additional coating reserve, but it does not automatically increase the allowable operating temperature. Base steel, atmosphere, berbasikal haba, pemprosesan, and required service life also matter.

Apakah perbezaan antara AS120 dan AS150?

The primary difference is the specified coating mass, with AS150 representing a heavier coating level than AS120. The appropriate selection depends on the applicable standard and the required protection level.

Should the inside of an aluminized tube also be coated?

If the internal surface is exposed to hot gas, condensate, combustion products, or another corrosive medium, keperluan salutan dalaman hendaklah dinyatakan dengan jelas. Jangan menganggap bahawa sebutan salutan luaran secara automatik menerangkan permukaan dalaman.

Apakah maklumat yang perlu saya berikan kepada pembekal tiub keluli alumin?

Sediakan gred keluli asas, dimensi tiub, panjang, jenis salutan dan jisim, internal coating requirement, suhu operasi, atmosphere, keperluan pemprosesan, kuantiti, piawaian yang berkenaan, dan keperluan dokumentasi pemeriksaan.

Kongsi siaran ini