Tubo de aço aluminizado DX54D+AS: Nota, Revestimento & Guia de solicitação de cotação

Tubo de aço aluminizado DX54D+AS: Nota, Revestimento & Guia de solicitação de cotação

DX54D+AS é frequentemente descrito no mercado como “tubulação aluminizada,” mas esta descrição é tecnicamente incompleta. De acordo com EN 10346, DX54D+AS refers to a continuously hot-dip-coated flat steel product: DX54D defines the formability of the steel substrate, while +AS denotes an aluminum-silicon coating system. Finished aluminized tubes are typically manufactured by forming and welding this coated flat steel. Portanto, tube specifications must separately define the substrate grade, coating mass, processo de fabricação, and dimensional requirements for the finished tube.

1. First Correction: DX54D+AS Is Not a Tube Grade

This distinction is critical when preparing a request for quotation (RFQ) or technical data sheet. EM 10346 covers continuously hot-dip-coated flat steel products for cold forming, but it does not establish “DX54D+AS tubing” as an independent tube or pipe grade. [Classe de tubo DX54D+AS ou aço plano revestido? Guia de especificações]

Specification LevelWhat It DefinesProcurement Question
DX54DCold-forming steel substrate and mechanical propertiesIs the substrate actually DX54D?
+COMOHot-dip aluminum-silicon coatingWhat coating mass is required?
Tube StandardTube dimensions, tolerâncias, requisitos de formação e soldagemWhich tube standard and manufacturing process apply?

Procurement Rule: Never specify only “DX54D+AS tube.” A complete technical purchase order should identify the substrate grade, coating designation and mass, tube manufacturing standard, dimensões, tolerâncias, requisitos de soldagem, and inspection documentation.

Material Numbers: 1.0306 e 1.0952

As European standards evolve, older drawings and supplier documents may contain different material numbers associated with the DX54D material designation. Historical documents may reference 1.0306, whereas current documentation may identify DX54D using material numbers such as 1.0952 under updated EN 10346-related documentation. [1.0306 ou 1.0952? Transição do número do material DX54D explicada]

When the material number on an older drawing differs from that on a current mill certificate, procurement teams should not automatically treat the materials as different grades. Em vez de, verify the applicable edition of the standard and, where necessary, request a formal equivalence statement or material identification declaration.

2. Decoding DX54D+AS

SymbolMeaningTechnical Significance
DXCold-forming steel designationIdentifies a steel family designed for forming and continuous hot-dip coating
54Deep-drawing grade designationIndicates enhanced formability within the DX steel family compared with general forming grades
DDesignation for flat steel products intended for hot-dip coatingDistinguishes this material designation from other steel product and coating systems
+Coating designator separatorSeparates the substrate grade from the coating designation
COMORevestimento de alumínio-silícioIdentifies an aluminum-based coating system designed to provide resistance to high-temperature oxidation

The same DX54D substrate can be combined with several different coating systems, including zinc, zinc-iron, zinc-aluminum, zinc-magnesium, aluminum-zinc, and aluminum-silicon coatings. Portanto, replacing +COMO with another coating designation is not simply a cosmetic substitution. It changes the coating system and may affect the finished material’s corrosion resistance, resistência ao calor, and processing characteristics. [+Revestimento AS vs +Z: Guia de alumínio-silício vs aço zinco]

GB/T 36399 hot-dip aluminum-silicon coated steel tubeGB/T 36399 tubo de aço aluminizado

3. DX54D Mechanical Properties: Why It Is a Deep-Drawing Steel

For procurement purposes, the deep-forming performance of DX54D should be evaluated using multiple mechanical indicators rather than elongation alone. Typical requirements include tensile strength, alongamento, plastic strain ratio, and work-hardening behavior, with applicable thickness corrections determined in accordance with the relevant standard. [r90 vs n90 na formação de chapas metálicas de estampagem profunda]

PropriedadeTypical DX54D+AS RequirementsProcurement Significance
Força de rendimento, ReApproximately 120–220 MPa*Indicates a low-strength substrate with high formability
Resistência à tracção, RmApproximately 260–350 MPaDefines the tensile strength range of the forming-grade steel
Alongamento, A80≥34%*Represents overall deformation capacity
r90≥1.4*Indicates resistance to excessive sheet thinning during forming
n90≥0.18*Indicates work-hardening behavior and strain distribution

*Applicable requirements and permitted values must always be verified against the exact edition of the standard, product thickness, surface quality requirements, and contractual specifications. [a80 r90 n90: Por que os requisitos de estampagem profunda de calibre fino são relaxados]

[Garantia de aço de seis meses: A folha envelhecida ainda pode ser carimbada?]

Thickness Corrections Must Be Specified in the Contract

Formability requirements for thin-gauge material may need to be adjusted. This is particularly important when purchasing material thinner than approximately 0.70 milímetros. If a specification states only “r90 ≥ 1.4” without identifying the applicable thickness correction, the supplier and buyer may apply different acceptance criteria to the same coil.

Faixa de espessuraA80 Adjustmentr90 Adjustmentn90 Adjustment
0.50 ≤ t < 0.70 milímetros−2 percentage points−0.2−0.01
0.35 ≤ t < 0.50 milímetros−4 percentage points−0.4−0.03
t < 0.35 milímetros−7 percentage points−0.6−0.04
1.50 < t ≤ 2.00 milímetros-−0.2-
t > 2.00 milímetros-−0.4-

The practical lesson is straightforward: never copy thin-gauge formability requirements directly from a general DX54D datasheet without checking the provisions applicable to the specific thickness.

Aluminized steel tube under ASTM A463, JIS G3314 and EN 10346 padrõesAluminized steel tubes for sale

4. Composição Química: Distinguishing the Steel Substrate from the Coating

Para DX54D, chemical composition requirements apply to the steel substrate, not the aluminum-silicon coating. Typical maximum values for the substrate include the following:

CEMnPSAl
≤0.12%≤0.50%≤0.60%≤0.10%≤0.045%≤0.30%

A common specification error is to see a silicon limit for the substrate and assume that it describes the coating composition. It does not. Silicon in the substrate’s chemical composition and silicon used in the aluminum-silicon coating belong to different metallurgical systems and must be evaluated separately.

5. What Does +AS Mean?

The +AS coating is an aluminum-silicon alloy coating, not a pure aluminum coating. Industrial aluminum-silicon coatings typically contain several percent silicon, with compositions containing approximately 10% silicon widely used. This coating system is designed to provide resistance to high-temperature oxidation while maintaining good adhesion and processability.

Tipo de revestimento

Uses an aluminum-silicon alloy rather than pure aluminum.

Typical Silicon Content

Approximately 5–11% silicon in common industrial formulations, depending on the specification.

Common Coating Designations

AS060, AS080, AS100, AS120, and AS150 are commonly used designations.

Aplicações Típicas

High-temperature components, exhaust-related products, equipamento de aquecimento, and other heat-exposed parts.

AS120 and ASTM A463 Type 1: Compare Coating Mass, Not Just Standards

EN and ASTM coating standards use different designation systems and units. Under the applicable EN coating system, AS120 denotes a nominal total coating mass of 120 g/m² across both surfaces. Tipo ASTM A463 1 uses designations expressed in ounces per square foot, such as T1-13, T1-25, T1-40, and T1-60. [Comparação de padrões de aço revestido EN ASTM JIS ISO Al-Si]

EN Coating DesignationNominal Total Coating MassApproximate ASTM Type 1 Comparação
AS06060 g/m²Below T1-25
AS08080 g/m²Close to the T1-25 range
AS120120 g/m²Close to T1-40, approximately 122 g/m²
AS150150 g/m²Between T1-40 and T1-60

Important: These are comparison values, not automatic declarations of material equivalence. The coating chemistry, test method, minimum values, designation rules, and application requirements must still be verified against the applicable standard. [Guia de revestimento AS060 vs AS080 vs AS100 vs AS120 vs AS150]

AS120 Coating Thickness: A Useful Engineering Estimate

If a total coating mass of 120 g/m² is distributed equally across two surfaces, each side accounts for approximately 60 g/m². Using an approximate density of 2.7 g/cm³ for an aluminum-based coating gives a theoretical single-side thickness of roughly 22 μm. This calculation is intended as an engineering estimate only. Actual coating thickness and distribution should be established using the applicable coating-mass test method and supplier documentation.

6. Deep Drawing: Why DX54D Is Suitable for Complex Forming

DX54D is intended for demanding cold-forming applications. Its forming behavior depends on the combined effects of elongation, plastic anisotropy, and work-hardening characteristics.

IndicatorWhat It ControlsWhy It Matters in Tube Production
A80Overall elongation capacitySupports forming without premature tensile fracture
r90Resistance to localized thinningImportant during deep drawing and severe cross-sectional deformation
n90Work-hardening behaviorInfluences how deformation is distributed throughout the forming zone

Another procurement consideration is resistance to stretcher strains. Surface strain marks can become a quality issue for components where appearance is important. For deep-drawing applications, material age should therefore be managed alongside mechanical properties and surface-quality requirements.

Where a supplier provides a defined aging or surface-quality guarantee period, the contract should state that requirement explicitly. Older stock should not automatically be considered equivalent to freshly produced material simply because the nominal grade remains unchanged.

7. The Critical Issue in Tube Manufacturing: Coating vs. Soldagem

Converting coated flat steel into tubing introduces a processing challenge that does not arise in exactly the same way when the product remains flat sheet: the aluminum-silicon coating interacts with the welding process.

Manufacturing StagePotential IssueProcurement Requirement
Welding ZoneThe coating may affect weld-pool behavior and weld qualityDefine the welding procedure and treatment of the weld zone
Método de soldagemProcess parameters must account for the coated steel substrateSpecify a qualified welding procedure and applicable consumables
Post-Weld ProtectionCoating removed or affected by heat may leave areas with reduced protectionDefine local protection or coating-repair requirements
Tube FormingSevere bending or expansion may place stress on the coatingVerify coating adhesion after forming
Cut EdgesExposed steel edges have less coating protectionSpecify edge condition and any required sealing or protection

Engineering Focus: For welded aluminized tubing, substrate selection is only one part of the corrosion-performance equation. The weld zone, cut edges, forming radius, and post-processing protection can determine the actual service performance of the finished tube.

8. Cross-Standard Comparison: Do Not Match Designations by Name Alone

SystemPadrãoTypical DesignationProcurement Note
EuropeanEM 10346DX54D+ASCoated flat steel product; the tube standard must be specified separately
Historical EuropeanEarlier EN specificationsDX54D+AS with historical material referencesOlder drawings should be checked against the current edition of the applicable standard
AmericanASTM A463/A463MTipo 1 Al-Sim; T1 coating designationsTipo 1 e tipo 2 are different coating systems
JapaneseJIS G 3314SA1C / SA1D / SA1EVerify the grade, coating mass, e aplicação pretendida
InternationalISO 5000Al-Si-coated cold-rolled carbon steel flat productsCheck the exact mechanical and coating requirements

The correct sequence for cross-standard comparison is substrate grade → coating chemistry → coating mass → mechanical requirements → dimensions → test method. A Type 1 Al-Si coating should not be considered interchangeable with a Type 2 pure-aluminum coating simply because both are described as aluminized steel.

9. Typical Applications and Selection Limitations

Automotive Exhaust Components

Suitable for applications requiring formability combined with resistance to high-temperature oxidation and atmospheric corrosion.

Aluminized Tubes and Fittings

Useful where coated steel tubing is required for exhaust systems, equipamento de aquecimento, or other temperature-exposed applications.

Equipamento de aquecimento

Applicable to selected oven, forno, heat-shield, and heat-exchanger components.

HVAC and Industrial Enclosures

Can combine cold-forming capability with atmospheric corrosion resistance in selected applications.

When Should DX54D+AS Be Reconsidered?

  • Extremely high service temperatures: Verify the actual continuous and cyclic operating temperatures rather than relying on generic statements about coating temperature resistance.
  • Severe chloride or chemical exposure: Evaluate the complete corrosion environment and compare alternative material systems.
  • Primary load-bearing structures: The low-strength deep-drawing substrate is not automatically suitable for structural applications requiring high yield strength.
  • Highly visible surfaces: Establish surface-quality, formando, and weld-zone requirements before production.
  • Severe post-forming operations: Confirm coating adhesion and the permissible forming radius before selecting the coating mass.

10. DX54D+AS Tube Specification: Complete RFQ Checklist

A professional aluminized tube specification should distinguish material requirements from finished-tube requirements. The following checklist can be incorporated into an RFQ:

ItemRequired Information
1. SubstratoDX54D and the applicable EN 10346 designação
2. Revestimento+AS and the exact coating mass designation, such as AS060, AS080, AS100, AS120, or AS150
3. Coating-Mass ConventionClearly specify the total mass across both surfaces or the applicable alternative measurement convention
4. Propriedades MecânicasRe, Rm, A80, r90, and n90, including applicable thickness corrections
5. Composição QuímicaHeat analysis and material certificate requirements
6. Tube DimensionsOutside diameter, espessura da parede, comprimento, ovality, and dimensional tolerances
7. Método de fabricaçãoFormando, soldagem, and any subsequent tube-forming operations
8. Weld RequirementsWelding procedure, weld inspection, and treatment of the coated zone
9. Edge ProtectionProtection requirements for cut edges and weld areas
10. Qualidade de SuperfícieSurface class, permissible defects, and coating adhesion requirements
11. Material AgeApplicable forming-quality or aging-guarantee requirements
12. Inspection DocumentationMechanical, químico, coating-mass, adesão, e registros de inspeção dimensional

11. Three Contract Clauses That Prevent Common Disputes

Dispute 1 — Thin-Gauge Material Fails a Formability Test.
Cause: The contract copied a nominal r90 or n90 requirement without incorporating the applicable thickness adjustment.

Dispute 2 — Coating Mass Does Not Match Between Supplier and Buyer.
Cause: One party interprets the value as the total coating mass across both surfaces, while the other uses a different unit or measurement convention.

Dispute 3 — Older Stock Develops Forming or Surface-Quality Problems.
Cause: Material age was not controlled, even though the application requires reliable deep drawing and freedom from surface strain marks.

The simplest way to prevent these disputes is to attach the applicable standard requirements and exact acceptance methods to the purchase order rather than relying on a short material designation.

12. Teda Ganghua Support for Aluminized Steel Coil and Tube Projects

Teda Ganghua can support procurement teams sourcing coated steel for exhaust, aquecimento, Hvac, aparelho, and tube-manufacturing applications. For a DX54D+AS project, procurement can be organized around the substrate grade, coating designation, coating mass, grossura, largura, formando requisitos, dimensões do tubo, processo de soldagem, and inspection documentation.

For projects in which coated steel is purchased in coil form and subsequently converted into welded tubing, it is particularly important to evaluate the flat-product specification together with the downstream tube-manufacturing process. Teda Ganghua can coordinate material requirements for bobina de aço aluminizado applications and help procurement teams define the required coating grade, dimensões, formando requisitos, and documentation before order confirmation.

This approach reduces the risk of receiving material that matches the stated material designation but does not meet the actual requirements of tube production. For engineering and procurement teams, the objective should always be to establish a complete material-to-tube specification rather than simply copying a single grade designation into the purchase order.

13. Final Engineering Takeaways

DX54D+AS combines a low-carbon steel substrate with a hot-dip aluminum-silicon coating and is intended for deep-forming applications. Its value lies in the combination of formability and high-temperature coating performance, but the designation itself does not define the finished tube. [Conversão de Massa de Revestimento: Explicação de lado único vs lado duplo]

To ensure reliable procurement, divide the specification into four levels: DX54D substrate → +AS coating → coating mass → finished-tube manufacturing standard. Then add thickness-dependent mechanical requirements, controles de soldagem, edge protection, surface acceptance criteria, material-aging requirements, and inspection documentation. [Soldagem de tubos de aço aluminizado: Remoção e reparo de revestimento]

[Prevenção de ferrugem em tubos de aço aluminizado em soldas e bordas cortadas]

The most important procurement rule is simple: match the complete technical specification, not just the material code.

[Aço Aluminizado vs Aço Inoxidável Ferrítico para Sistemas de Exaustão]

Perguntas frequentes

Is DX54D+AS a tube grade?

Não. It refers to a continuously hot-dip aluminum-silicon-coated flat steel product under the relevant EN standard. Finished aluminized tubes are manufactured from coated flat steel, so the tube standard and manufacturing requirements must be specified separately.

What does +AS mean?

+AS denotes an aluminum-silicon coating, not a pure aluminum coating. The coating chemistry and coating mass must be specified separately from the DX54D substrate grade.

What is AS120?

AS120 is a coating designation indicating a nominal coating mass of 120 g/m² under the applicable EN coating system, generally referring to the combined mass on both surfaces. Its coating mass is approximately comparable to ASTM A463 Type 1 T1-40, but the two designations should not be considered fully equivalent.

Why are thickness corrections important for DX54D?

Deep-forming properties, including elongation, r90, and n90, may be subject to thickness-dependent adjustments. The applicable corrections should be included in the procurement specification so that the supplier and buyer apply the same acceptance criteria.

What is the main issue when converting DX54D+AS into tubing?

The welding and subsequent forming operations must be compatible with the aluminum-silicon coating. The weld zone, cut edges, e áreas fortemente formadas podem exigir medidas de processamento específicas e proteção localizada para manter o desempenho de serviço pretendido.

O DX54D+AS pode ser usado para sistemas de escapamento automotivo??

Pode ser adequado para componentes selecionados de exaustão e de alta temperatura quando sua conformabilidade e desempenho do revestimento de alumínio-silício atendem à temperatura real, corrosão, soldagem, e requisitos de vida útil. O ambiente operacional completo deve ser avaliado antes que o material seja aprovado.

 

Compartilhe esta postagem